Clothing Manufacturer_Clothing Factory clothing manufacturers News Common problems and countermeasures in water and oil repellent finishing (3)

Common problems and countermeasures in water and oil repellent finishing (3)



Water stains occur 1. Reason: ⑴The working fluid has poor stability. This can be determined by observing the surface layer of the working fluid after high-speed stirring and whethe…

Water stains occur
1. Reason:
⑴The working fluid has poor stability. This can be determined by observing the surface layer of the working fluid after high-speed stirring and whether there is scum on the roll.
⑵ Malignant bubbles may occur. This can be touched by hand. If it agglomerates and turns into scum, it is a malignant bubble.
2. Main countermeasures:
⑴ Pay attention to control the temperature of the working fluid not to exceed 35C.
⑵ When malignant bubbles are found, add stabilizer (isopropyl alcohol).

⑶Use within the shelf life.

Extended reading: https://www.yingjietex.com/product/1200D-Polyester -OXFORD-Fabric.html
Extended reading: https://www.alltextile. cn/product/product-9-995.html
Extended reading: https:/ /www.alltextile.cn/product/product-36-562.html
Extended reading:https://www.yingjietex.com/product/Full-dull-Nylon-dobby-checked-taffeta-Fabric.html
Extended reading:https://www.alltextile.cn/product/product-32-236.htm

 